http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CA-1168480-A

Outgoing Links

Predicate Object
assignee http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_0e7b522b71fd001f1a633fd8563b2a3e
classificationCPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C22C38-08
classificationIPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C22C38-08
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B22D11-10
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C22C38-00
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C22C33-04
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B22D11-00
filingDate 1981-07-23-04:00^^<http://www.w3.org/2001/XMLSchema#date>
grantDate 1984-06-05-04:00^^<http://www.w3.org/2001/XMLSchema#date>
inventor http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2d5354674a32685f3a18f3f268e6e91d
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5b1353c8fa83881e2e84ea8bd417f0ec
publicationDate 1984-06-05-04:00^^<http://www.w3.org/2001/XMLSchema#date>
publicationNumber CA-1168480-A
titleOfInvention Prevention method of surface crackings on ni- containing, continuously cast steel products
abstract ABSTRACT OF THE DISCLOSURE A method of preventing surface cracking of Ni-containing, continuously cast steel products. The chemical composistion of Ni-containing molten steel is adjusted, and the molten Ni steel is continuously cast without limitation on the casting condition and the cooling condition; the continuously east product reveals no surface trackings an; the product is imparted with excellent properties for service at low temperatures.
priorityDate 1980-07-23-04:00^^<http://www.w3.org/2001/XMLSchema#date>
type http://data.epo.org/linked-data/def/patent/Publication

Incoming Links

Predicate Subject
isDiscussedBy http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID426228520
http://rdf.ncbi.nlm.nih.gov/pubchem/anatomy/ANATOMYID163112
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID16723172
http://rdf.ncbi.nlm.nih.gov/pubchem/taxonomy/TAXID163112

Total number of triples: 21.