http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CA-1118483-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c391364e0741043fad9d4ca5347ce1a6 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03G9-08702 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03G9-08715 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03G9-08737 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03G9-08731 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03G9-08717 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03G9-08724 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03G9-087 |
filingDate | 1978-05-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 1982-02-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_558e1374394282c8e2bee312aecb4eb6 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_350de655e3acccd79b042f9b6f455489 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1cf8f35a32eb7e721f19b9e3ba0b1e70 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5d732f3315f24f5251e4747da2e522da http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3a125ba3598a2c1f9b160479144750c2 |
publicationDate | 1982-02-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CA-1118483-A |
titleOfInvention | Developer for electrostatic images and process for preparation thereof |
abstract | Abstract of the Disclosure A developer for electrostatic images comprising a binder medium and a pigment dispersed in the binder medium is disclosed. This binder medium comprises (A) a thermoplastic or rubbery polymer containing a member selected from the group consisting of a halogen atom and a nitrile group at a concentration of at least 100 milliequivalents per 100 g of the polymer and (B) a binder having a melting temperature lower than that Or the polymer (A) at an (A)/(B) mixing weight ratio of from 1/20 to 1/1, The halogen- or nitrile-containing polymer (A) is present in the form of fine particles dispersed in the continuous phase of the binder (B). This developer has good flowability and charge charac-teristics at the developing step and shows an excellent offset-preventing effect at the fixing step. |