abstract |
interior item for cars with reduced odor. the present invention relates to automotive interior article comprising a polypropylene composition having a melting flow rate mfr2 (230 ° c) of 2.0 to 80.0 g / 10min, said polypropylene composition comprises (a ) at least 25% by weight of a heterophasic polypropylene (h-pp1), (b) 10,000 to 550,000 ppm of inosilicate, (c) 1000 to 5,000 ppm of phenolic antioxidants, and where said heterophasic polypropylene (i) comprises a polypropylene matrix and an elastomeric copolymer, said elastomeric copolymer comprises propylene and eylene units and / or c4 to c20 (alpha) -olefin (ii) has a comonomer content of 8 to 30% by weight based on said heterophasic polypropylene , said comonomer is ethylene and / or at least one c4 to c20 (alpha) -olefin, and (iii) has a cold soluble xylene content (xcs) measured according to the iso 6427 method from 15.0 to 40 , 0% by weight based on heterophasic polypropylene. |