http://rdf.ncbi.nlm.nih.gov/pubchem/patent/BR-PI0618714-A2
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_0823a228ec4ef9871401a999c47d01d6 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C06B21-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C06B21-0025 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C06B21-0058 |
filingDate | 2006-11-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9d7630cee1921d533ad3882094c5420e |
publicationDate | 2013-01-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | BR-PI0618714-A2 |
titleOfInvention | Semi-continuous two-component methods for obtaining a composite explosive charge of polyurethane matrix |
abstract | METHOD OF TWO SEMI-CONTINUOUS COMPONENTS FOR OBTAINING A COMPOSITE EXPLOSIVE POLYURETHANE MATRIX LOAD The invention relates to a semi-continuous two-component method for obtaining a composite explosive charge consisting of a solid charged polyurethane matrix, which is charge in the form of a powder and comprising at least one organic nitro explosive. Said method includes the following successive steps: obtaining a pasty explosive composition consisting essentially of the following constituent ingredients: a polio prepolymer, a polysocyanate monomer, a plasticizer and a solid powdered form comprising at least an organic nitro explosive, continuously mixing a pasty component A 'and a liquid component B' prepared individually from said constituent ingredients; introducing said composite explosive composition into a mold; and thermally crosslinking said composition in said mold. The invention is characterized in that said liquid component B 'comprises from 90 to 99% by weight of said polyisocyanate monomer; said component A 'comprises the entire polyol polymer, the total powdered solid filler and the remainder 1 to 10% by weight of the polyisocyanate monomer; the plasticizer being distributed indistinctly between components A 'and B'; wherein the continuous mixing of said components A 'and B' is such that the mass ratio of component A '/ component B' is constant, ranging from 95.05 / 4.95 to 99.5 / 0.45. Said method constitutes a particularly interesting improvement of the method according to EP-A-1 133015. |