http://rdf.ncbi.nlm.nih.gov/pubchem/patent/BR-PI0610631-A2
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_9b449501522aa74c4e7883dcee4f8200 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2325-06 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J9-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J9-224 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J9-0066 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J9-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J9-224 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J7-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J9-00 |
filingDate | 2006-04-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_36ff2a7f3885c8f131f19e43988f256b http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_465783a2739b7a62267c385638d9f6d5 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_be8c4107843167d51e799cbd4d0d6858 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_516400b4a5074167413e8190b524ee9b |
publicationDate | 2010-07-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | BR-PI0610631-A2 |
titleOfInvention | process for improving the insulation capability of expanded vinyl aromatic polymers and products obtained in this way |
abstract | Patent of Invention: Process for Improving the Insulation Capacity of Expanded Aromatic Vinyl Polymers and the Products Obtained THIS WAY. The present invention relates to a process for improving the expanded vinyl aromatic polymer insulation capability comprising: 1) preparing expandable vinyl aromatic polymer beads containing 1 to 10% by weight calculated on the polymer of a blowing agent comprised in the polymeric matrix and 0.001 to 25% by weight, calculated with respect to polymer (a), of an atherman additive comprising carbon black evenly distributed in the polymeric matrix; 2) treating the surface of the beads prior to deposition of the cover with a liquid lubricating agent; and 3) heat treat the beads with hot air at a temperature ranging from 30 to 60 ° C. |