http://rdf.ncbi.nlm.nih.gov/pubchem/patent/AU-2019479700-A1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_5ede8ab2ac83cad6c4b978986be109cd |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-06 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-06 |
filingDate | 2019-12-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4ceefc1fb807a24912697673df029e10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7932870dfa801020d1a0e0a8dcc2639e http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_df6a0a2ed62b70a7442ab9747c5543c6 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6ba32a1977c09d13e2aadde9f690861b http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_bc4dc98b47eb570080eba352ea2f8b67 |
publicationDate | 2022-07-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | AU-2019479700-A1 |
titleOfInvention | Flame-retardant wood-plastic surface layer composite, and method for preparing wood-plastic composite material having flame-retardant wood-plastic surface composite |
abstract | Disclosed are a flame-retardant wood-plastic surface layer composite, and a method for preparing a wood-plastic composite material having the flame-retardant wood-plastic surface layer composite, relating to the technical field of wood-plastic materials. Raw materials of the flame-retardant wood-plastic surface layer composite specifically comprise, in parts by mass, the following components: 10 to 50 parts of a high-density polyethylene, 10 to 50 parts of polypropylene, 10 to 50 parts of an ethylene-acrylic acid copolymer, 10 to 50 parts of a filler, 10 to 30 parts of a flame retardant, 0.1 to 0.5 part of an anti-ultraviolet agent, 0.1 to 0.5 part of an antioxidant, 0.5 to 8 parts of a color powder, 0.1 to 1 part of an anti-mildew agent, 0.1 to 3 parts of a lubricant, and 0.5 to 6 parts of a layered silicate. The present invention has fireproof and flame retardant effects, and the bonding strength between a wood-plastic flame-retardant surface layer and a core layer is high. |
priorityDate | 2019-12-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 69.