http://rdf.ncbi.nlm.nih.gov/pubchem/patent/AU-2019410391-A1

Outgoing Links

Predicate Object
assignee http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_f506d01d7c64b8a38040974fa9a16821
classificationCPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D04H1-641
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D04H1-4226
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D04H1-643
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D04H1-642
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C25-1095
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C25-24
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C25-146
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D04H1-645
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D04H1-655
classificationIPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03C25-1095
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G01N33-38
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D04H1-645
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D04H1-64
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03C25-146
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03C25-24
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D04H1-4226
filingDate 2019-12-19-04:00^^<http://www.w3.org/2001/XMLSchema#date>
inventor http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ad4a10df8224bc4178ff08fc59831009
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_cdadc1a847eab432d965128f5a698992
publicationDate 2021-07-08-04:00^^<http://www.w3.org/2001/XMLSchema#date>
publicationNumber AU-2019410391-A1
titleOfInvention Method for adjusting the amount of dilution water of a sizing composition, and corresponding calculcating unit
abstract The invention relates to a method for manufacturing a mat of mineral fibres (F), wherein the fibres (F) are formed and a sizing composition obtained from mixing a binder composition with dilution water is applied to the fibres (F), the fibres impregnated with the sizing composition are collected on an open-worked receiving device (52) provided with a fibre-receiving surface and, under the surface, at least one suction sheath (54), and the mat is thermally treated. The method according to the invention comprises a step of determining an optimal amount of dilution water according to the humidity of the air on the fiberising station (12), the humidity of the air drawn in and the flow of air drawn into the at least one suction sheath (54), and the amount of water desired in the mat at the outlet of the receiving chamber (50), and a step of adjusting the amount of dilution water according to the optimal amount thus determined.
priorityDate 2018-12-21-04:00^^<http://www.w3.org/2001/XMLSchema#date>
type http://data.epo.org/linked-data/def/patent/Publication

Incoming Links

Predicate Subject
isDiscussedBy http://rdf.ncbi.nlm.nih.gov/pubchem/gene/GID63974
http://rdf.ncbi.nlm.nih.gov/pubchem/gene/GID11922
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID419578879
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID419512635
http://rdf.ncbi.nlm.nih.gov/pubchem/protein/ACCQ08DI0
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID172281
http://rdf.ncbi.nlm.nih.gov/pubchem/protein/ACCQ4R5G6
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID962
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID452697243
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID168365
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID415712566
http://rdf.ncbi.nlm.nih.gov/pubchem/protein/ACCP48986
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID76173
http://rdf.ncbi.nlm.nih.gov/pubchem/protein/ACCQ96NK8

Total number of triples: 40.