abstract |
The present invention relates to an inoculant for the manufacture of cast iron with spheroidal graphite, said inoculant comprises a particulate ferrosilicon alloy consisting of between 40 and 80 % by weight of Si; 0.02-8 % by weight of Ca; 0-5 % by weight of Sr; 0-12 % by weight of Ba; 0-15 % by weight of rare earth metal; 0-5 % by weight of Mg; 0.05-5 % by weight of Al; 0-10 % by weight of Mn; 0-10 % by weight of Ti; 0-10by weight of Zr; the balance being Fe and incidental impurities in the ordinary amount, wherein said inoculant additionally contains, by weight, based on the total weight of inoculant: 0.1 to 15 % of particulate Bi |