abstract |
A plastic film formed of a layer and at least one skin layer, with the formulation: (i) about 10% to about 70% of a polyethylene resin (e.g. LLDPE, MDPE, HDPE, PERT) of fractional melt index (<0.6 gr/10 min, 190°C, 2.16 kg/min) and a density ranging from 0.910 to 0.960 5 g/cm3; (ii) about 30% to 90% of a LDPE resin of fractional melt index (<1 gr/10 min, 190°C, 2.16 kg/min) and a density from 0.910 to 0.960 g/cm |