Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_781c429e4e20536916ff74dcbe1b5417 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02P10-20 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C22B3-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C22B3-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C22B3-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C22B15-0065 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C22B15-0095 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C22B15-0063 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C22B15-0071 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C22B15-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C22B3-26 |
filingDate |
2016-03-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
2018-07-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3a2745225378fc9cfec5ac3224c7e256 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ba0b42cf59680fb3b7d815cfb777b3e4 |
publicationDate |
2018-07-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
AU-2016234208-B2 |
titleOfInvention |
Method of leaching copper from copper sulfide ore and method of evaluating iodine loss content of column leaching test of the copper sulfide ore |
abstract |
A method of leaching copper from a copper sulfide ore which includes adding a potential adjustment agent for lowering a potential of a leaching solution obtained after leaching copper from the copper sulfide ore by using iodide ion and iron (III) ion, the leaching solution being stored in a tank for storing the leaching solution. |