Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_be2258efa1dd0212d91e87b0487f4ede |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02W30-91 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2103-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2103-12 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B28-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B18-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09K8-467 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B14-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B18-146 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B24-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B40-0658 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B22-062 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B22-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/E21B33-13 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/E21B33-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B22-082 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/E21B33-13 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09K8-42 |
filingDate |
2014-10-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8ffd0e4dafcfa45f1e23a49bc3ef722b http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9bc43700f7b63f4eade09dc374b77431 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_35fef90cb8e92b2b123b5297095cd1d7 |
publicationDate |
2017-03-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
AU-2014408279-A1 |
titleOfInvention |
Extended-life calcium aluminate cementing methods |
abstract |
Methods of using extended-life cement compositions are disclosed. A method comprises providing an extended-life cement composition comprising calcium-aluminate cement, water, and a cement set retarder. The method additionally comprises mixing the extended-life cement composition with a cement set activator to activate the extended-life cement composition. The method further comprises Introducing the activated extended-life cement composition into a subterranean formation and allowing the activated extended-life cement composition to set in the subterranean formation; wherein the activated extended-life cement composition has a thickening time of greater than about two hours. |