http://rdf.ncbi.nlm.nih.gov/pubchem/patent/AU-2013245537-B2
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_49f5a779eff1897763fbeb8273e8ab99 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J3-24 |
filingDate | 2013-10-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2016-02-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_29a65291f9a5d69f4f58cda0f0c523f5 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_14e16ac3f4f64500ca721ed20180a846 |
publicationDate | 2016-02-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | AU-2013245537-B2 |
titleOfInvention | Method for producing heat shrinkable polyester film |
abstract | METHOD FOR PRODUCING HEAT SHRINKABLE POLYESTER FILM A method for producing a heat shrinkable polyester 5 film includes the following steps: (a) providing a polyester film that has a glass transition temperature (Tg) C; (b) preheating the polyester film at a preheating temperature ranging from (Tg+20) 'C to (Tg+30) C; (c) drawing the preheated polyester film 10 along a transverse direction which is perpendicular to a machine direction with a draw ratio ranging from 2.7 to 7.7; and (d) annealing the drawn polyester film at an annealing temperature ranging from (Tg-10) 0C to Tg0 C, followed by cooling to room temperature so as to obtain 15 the heat shrinkable polyester film. |
priorityDate | 2013-01-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |