Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_4a96e25d2dead80123fbb920e4a3c2cf |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B23K2101-04 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B23K37-003 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B23K35-3603 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B23K35-3602 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B23K35-362 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B23K20-023 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B23K20-028 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B23K20-165 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B23K20-002 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B23K35-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B23K35-3606 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B23K35-0244 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B23K20-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B23K20-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B23K35-362 |
filingDate |
2013-02-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
2016-09-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7d0c654bbf37a0fe17f95173d9cc28ae http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c3e658e11e32d9a3fe37fdf07a1c663f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7bc7bef3192e859c989c4ef7c6888a39 |
publicationDate |
2016-09-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
AU-2013224000-B2 |
titleOfInvention |
Method and machine for forge welding of tubular articles and exothermic flux mixture and method of manufacturing an exothermic flux mixture |
abstract |
A method of forge welding includes placing at least two components (1, 2) for welding together, adjacent each other and with an exothermic flux mixture (8) placed between the components. The exothermic flux mixture (8) is heated to initiate an exothermic reaction and the faying surfaces (12) of the two components are pressed together. The components being welded may be tubular, in particular pipes. Apparatus (20) for the method of forge welding and exothermic flux mixtures for the method of forge welding are also provided. |