Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_6b25e297fafe16fe675ead4710cd228a |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-31663 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L93-04 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D193-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D4-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D5-165 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D5-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D5-1618 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D133-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D143-04 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D193-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D5-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D133-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D143-04 |
filingDate |
2009-12-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
2012-11-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_11fc727e0db61476a640d048a1deb685 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_657ea0631a267dc6266c82d000456793 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ef1e4534d09629803f29106b4e4431ae http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_82576409f1b541633b9fdb09cba48db8 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8bcb2314d82e8abe88a321cec459b92b |
publicationDate |
2012-11-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
AU-2009327936-B2 |
titleOfInvention |
Antifouling coating composition, antifouling coating film formed using the composition, coated object having the coating film on the surface, and method of antifouling treatment by formation of the coating film |
abstract |
A composition for forming an antifouling coating film which, in seawater, can effectively have antifouling performance over long and has a small temperature dependence of coating film dissolution rate and which is highly safe for the environment. The antifouling coating composition is characterized by comprising (A) a triorganosilyl-ester-containing copolymer obtained from a mixture of (a) a triorganosilyl methacrylate monomer represented by general formula (1) (wherein R, R, and R are the same or different and each represents an α-branched C alkyl or phenyl) and (b) a methoxyalkyl methacrylate monomer represented by general formula (2) (wherein R represents a C alkylene), the content of the monomer (a) in the mixture being 45-65 wt.% and the total content of the monomer (a) and the monomer (b) in the mixture being 80 wt.% or higher, and (B) at least one copper salt selected from the copper salt of rosin and the copper salts of rosin derivatives. |