Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_5e5dac8eb9134a5455a6a178d41373e5 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C22B15-0089 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02P10-20 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C22B23-043 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C22B23-0453 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C22B23-0461 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C22B3-44 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C22B3-42 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C22B23-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C22B3-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C22B3-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C22B3-42 |
filingDate |
2008-05-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
2012-07-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3dee522dd4fcef7848a91d2b2fbd4239 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ebe3e05ef060b15416c09b197ff4d20a http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5c0286ee4dadd8b404e6f38480d2055a http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c5bba3b0450fe89ac593ee111108f4f7 |
publicationDate |
2012-07-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
AU-2008251010-B2 |
titleOfInvention |
Nickel recovery from a high ferrous content laterite ore |
abstract |
A process for the recovery of nickel and/or cobalt from laterite or partially oxidised lateritic ores having a substantial proportion of the iron present in the ferrous state, said process including the steps of : a) providing a laterite or partially oxidised laterite ore wherein a substantial proportion of the iron present in the ore is in the ferrous state; b) acid leaching the ore to provide a product leach solution containing at least ferrous iron, nickel and cobalt together with acid soluble impurities; and c) recovering the nickel and cobalt from the product leach solution with a selective ion exchange resin in an ion exchange process leaving the ferrous iron and other acid soluble impurities in the raffinate. |