http://rdf.ncbi.nlm.nih.gov/pubchem/patent/AU-2006231015-B2
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_9eedc17b5bb7a0d4162cb5aa8c641c0c |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L25-10 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L21-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J9-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L7-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L9-08 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L9-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J9-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L7-02 |
filingDate | 2006-03-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2012-11-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f162f7f61076b5f7fef6ea12f3a87383 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_333fb1c23f883271a81066709e25f3fd http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8dee677a2753f9bbb81f697d662c789f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4c4904cff34a96920bc1832a24677685 |
publicationDate | 2012-11-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | AU-2006231015-B2 |
titleOfInvention | New aqueous reinforced rubber dispersions and their use for making latex foams |
abstract | The present invention relates to an aqueous reinforced rubber dispersion comprising: a) 51 to 90 wt-% of base latex polymer particles; and b) 10 to 49 wt-% of reinforcing latex polymer particles comprising structural units of aromatic vinyl monomers and conjugated diene monomers, the reinforcing latex polymer particles having a single glass transition temperature (T) from -25°C to 28°C as measured by differential scanning calorimetry (DSC), whereby the weight percentages are based on the total weight of polymer particles in the rubber dispersion and the base latex polymer particles have a T as measured by DSC that is lower than the T of the reinforcing latex particles, to the use of the rubber dispersion for making latex foam, to a method for making latex foam and to an article comprising the latex foam obtained from the rubber dispersion of the present invention. |