http://rdf.ncbi.nlm.nih.gov/pubchem/patent/AT-514955-A4
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_fe28942c6ae06389f00c02ded2d5e6bc |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/F16C2240-60 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/F16C2223-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/F16C2202-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/F16C2223-60 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/F16C2220-20 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/F16C33-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/F16C33-125 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C23C14-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C23C14-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C23C14-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C23C14-32 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C23C14-24 |
filingDate | 2014-01-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_05c618e8d5ef7818c60b2321e9e15e1b |
publicationDate | 2015-05-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | AT-514955-A4 |
titleOfInvention | Method for producing a two-substance plain bearing |
abstract | The invention relates to a method for producing a two-substance plain bearing (1) according to which a metallic sliding layer (3) of at least two different particle types is deposited under reduced pressure on a planar, metallic substrate (8), wherein a first type of particle one Forming matrix with first grains and the second particle type embedded in the matrix grains of the metallic sliding layer (3), wherein the metallic sliding layer (3) with a layer thickness (4) of more than 250 microns and with a hardness of Vickers of less than 100 HV ( 0.025), and the metallic sliding layer (3) consists of a single layer in only one pass and with a maximum grain size of at least 90% of the first grains forming the matrix and with a maximum grain size of at least 90% of the incorporated grains of at most 1 and a maximum grain size of the remaining grains to 100% total grains of a maximum of 1.5 microns will be produced. |