http://rdf.ncbi.nlm.nih.gov/pubchem/patent/AT-270575-B
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_68b6f590ff7e5929ed3987a5f90fec3d |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D06M- |
filingDate | 1965-03-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 1969-05-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 1969-05-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | AT-270575-B |
titleOfInvention | Process for improving the properties, in particular the tear strength and tear strength, of textile fabrics consisting at least partially of cellulose fibers |
priorityDate | 1965-03-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links